Fastener Grade Selector: Which Grade Actually Survives the Joint

Over specification usually happens because corrosion and load get decided separately. Set both at once and see what genuinely satisfies both, and just as usefully, when nothing does.

Live selector

Set the Environment and Tensile Strength to Find a Fastener Grade

Choose a service environment and a minimum tensile strength and the matching grades, and the ones that fall short, update immediately.

The joint

The property class you need, in MPa. Common marks: A2-70/A4-70 = 700, A4-80 and class 8.8 = 800, class 10.9 = 1040, class 12.9 = 1220.

Why PREN

Pitting resistance equivalent number, %Cr + 3.3×%Mo + 16×%N. It is the standard single-number proxy for how a stainless resists chloride pitting. Higher is more resistant; it is not a strength figure and says nothing about load.

Options

Every grade against this joint

Corrosion resistance across the estate of common grades. The dashed line is the PREN this environment needs; bars left of it do not clear it. Coated carbon and alloy steels have no PREN, their corrosion life is the coating’s, specified separately under ISO 12944.

Where this stops and an engineer starts

This narrows a field. It does not qualify a joint. Galling on assembly, hydrogen embrittlement on high-strength plated parts, crevice geometry, galvanic pairing with the parent material, temperature and preload all decide real applications, and none of them is a single number. That conversation is what design assist engineering is for.

Where every figure on this page comes from
  • Strength: the published minimums for the named property class: ISO 3506-1 for stainless (A2-70/A4-70 = 700 MPa tensile, 450 MPa yield; A4-80 = 800 / 600) and ISO 898-1 for carbon and alloy steel (8.8 = 800 / 640, 10.9 = 1040 / 940, 12.9 = 1220 / 1100).
  • PREN: published values for the named alloy: 304 ≈ 19.6, 316 ≈ 24.2, duplex 2205 ≈ 34.8, super duplex 2507 above 40.
  • Environments: ISO 9223 atmospheric corrosivity categories, with the PREN thresholds general industry practice applies to them.

Duplex and super duplex rows carry a confirm the class flag because their fastener property classes vary by producer and by standard edition. The strength shown is a common supply, not a single standard minimum, confirm it before you specify it. No price appears anywhere on this page, because a real fastener price depends on size, volume, finish and lead time, and an invented one would be worse than none.

Explore the tools

Every Number on This Site Is One You Can Move

Bin Replenishment Simulator

Demand, lead time and service level in, safety stock and a simulated run out.

Grade and Environment Selector

Environment and load in, the grades that survive the joint out. You are here.

Cost of an Escaped Defect

PPM and catch rates in, the cost of a quality escape out.

Now get the number that is missing

You Have a Number. Now Get the One That Is Missing.

Everything on this page is modelled from the figures you entered. The piece price, the lead time and the tooling are ours to quote, and they are the numbers that turn this from an estimate into a decision. Send us the part, or the problem, and we will come back with both.

Prefer to talk it through?